In the manufacturing of metal components both wear and corrosion have to be considered. In particular, corrosion is a primary problem in the aeronautic field, where the aluminium alloys are affected by several corrosion typologies. Furthermore, nowadays carbon fibre reinforced plastics (CFRP) are finding an increasing use, but they can induce galvanic corrosion phenomena when coupled with aluminium alloys. To overcome this problem, corrosion resistant coatings are used on aluminium components. On these premises, the realization of a titanium coating on aluminium components could allow the coupling of CFRP and aluminium alloys, improving the corrosion resistance. Cold Spray Deposition is a recent technology to realize these coatings. This technology allows the production of near fully dense coatings on metallic surfaces. In many applications the coated aluminium sheets have to be machined (cut or drilled). Machining with conventional cutting methods leads to both tool wear and damages in the coating. Laser cutting represents a promising alternative: it does not involve any mechanical cutting force or tool wear and, thanks to the small laser beam spot, it allows to realize complex shapes. In this paper, laser cutting of an Al alloy sheet (0.6 mm thick) coated with Ti Alloy, was studied. The adopted laser source was a 150 W, lamp pumped Nd:YAG, specifically developed for micro-machining operations on metals. During the tests, the process parameters (cutting speed, pulse duration and entrance side) were changed and the kerf geometry was analysed as a function of the process parameters.

Laser Cutting of Aluminium Sheets with a Superficial Cold Spray Titanium Coating / Astarita, Antonello; Genna, Silvio; Leone, Claudio; MEMOLA CAPECE MINUTOLO, Fabrizio; Paradiso, Valentino; Squillace, Antonino. - 611-612:7(2014), pp. 794-803. (Intervento presentato al convegno Material Forming ESAFORM 2014 tenutosi a Espoo; Finland nel 7-9 May 2014) [10.4028/www.scientific.net/KEM.611-612.794].

Laser Cutting of Aluminium Sheets with a Superficial Cold Spray Titanium Coating

ASTARITA, ANTONELLO;GENNA, SILVIO;LEONE, CLAUDIO;MEMOLA CAPECE MINUTOLO, FABRIZIO;PARADISO, VALENTINO;SQUILLACE, ANTONINO
2014

Abstract

In the manufacturing of metal components both wear and corrosion have to be considered. In particular, corrosion is a primary problem in the aeronautic field, where the aluminium alloys are affected by several corrosion typologies. Furthermore, nowadays carbon fibre reinforced plastics (CFRP) are finding an increasing use, but they can induce galvanic corrosion phenomena when coupled with aluminium alloys. To overcome this problem, corrosion resistant coatings are used on aluminium components. On these premises, the realization of a titanium coating on aluminium components could allow the coupling of CFRP and aluminium alloys, improving the corrosion resistance. Cold Spray Deposition is a recent technology to realize these coatings. This technology allows the production of near fully dense coatings on metallic surfaces. In many applications the coated aluminium sheets have to be machined (cut or drilled). Machining with conventional cutting methods leads to both tool wear and damages in the coating. Laser cutting represents a promising alternative: it does not involve any mechanical cutting force or tool wear and, thanks to the small laser beam spot, it allows to realize complex shapes. In this paper, laser cutting of an Al alloy sheet (0.6 mm thick) coated with Ti Alloy, was studied. The adopted laser source was a 150 W, lamp pumped Nd:YAG, specifically developed for micro-machining operations on metals. During the tests, the process parameters (cutting speed, pulse duration and entrance side) were changed and the kerf geometry was analysed as a function of the process parameters.
2014
9783038351061
Laser Cutting of Aluminium Sheets with a Superficial Cold Spray Titanium Coating / Astarita, Antonello; Genna, Silvio; Leone, Claudio; MEMOLA CAPECE MINUTOLO, Fabrizio; Paradiso, Valentino; Squillace, Antonino. - 611-612:7(2014), pp. 794-803. (Intervento presentato al convegno Material Forming ESAFORM 2014 tenutosi a Espoo; Finland nel 7-9 May 2014) [10.4028/www.scientific.net/KEM.611-612.794].
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11588/581681
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 11
  • ???jsp.display-item.citation.isi??? 10
social impact